Application and problem analysis of hydroxypropyl methylcellulose in putty!

Neutral p创耀羟丙基甲基纤维素HPMC.jpgutty:

De pulverization: insufficient cementitious materials, insufficient water retention of cellulose and low calcium content of heavy calcium

Construction performance: improved by bentonite and starch ether

Empty drum; Caused by insufficient adhesion to the wall

Layering: interface processing

Strength: it can also be adjusted by calcium powder gradation

Grey calcium based putty:

The problems are hollowing, de pulverization and yellowing, poor workability, de pulverization, delamination, cracking and post thickening

De pulverization: insufficient cementitious materials, insufficient water retention of cellulose or insufficient addition, impure ash calcium

Poor construction performance: improved by bentonite and starch ether

Empty drum; Insufficient adhesion with the wall, resulting in appropriate addition of latex powder

Layering: interface processing

Yellowing: improper selection of cellulose

Cracking: the base course is cracked or the strength is too high, hard cracking, and the coating is too thick

Post thickening: the water absorption of heavy calcium is different, so it is recommended to select heavy calcium powder with zero water absorption or very low water absorption; Gray calcium contains undigested Gao.

Cement based putty:

The problems are hollowing, poor workability, de pulverization, delamination, cracking, insufficient water resistance and false coagulation

De pulverization: insufficient cementitious materials, insufficient water retention of cellulose or insufficient addition

Poor construction performance: improved by bentonite and starch ether

Empty drum; Due to insufficient adhesion with the wall, latex powder shall be added reasonably

Layering: interface processing

Yellowing: improper selection of cellulose

Insufficient water resistance: insufficient latex powder and insufficient cementitious materials

Cracking: the base course is cracked or the strength is too high, the hard cracking, the coating is too thick, and the holes are filled with putty

False coagulation: sodium gluconate can be added to prolong the operation time